Mallard Creek Polymers ROVENE® 6017 Styrene-Acrylic Emulsion

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers ROVENE® 6017 Styrene-Acrylic Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ROVENE® 6017 is a stiff, self-crosslinking styrene-acrylic copolymer emulsion with excellent water resistance and good mechanical stability.APPLICATIONS: ROVENE® 6017 is recommended for bonding nonwovens such as highloft webs, medical applications, and interlinings.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 44 - 46 %
44 - 46 %
Particle Size 0.20 µm
0.20 µm
pH 4.0 - 5.0
4.0 - 5.0
Brookfield Viscosity <= 100 cP
<= 100 cP
#2/20 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 35.0 °C
95.0 °F
Descriptive Properties Value Comments
Emulsifiers Anionic
Residual Monomer 0.02% Max