Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mallard Creek Polymers ROVENE® 6101 Styrene-Acrylic Emulsion

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers ROVENE® 6101 Styrene-Acrylic Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ROVENE® 6101 is a stiff, non-film forming high-gloss extending vehicle for flexographic and gravure inks and overprint varnishes. It is intended for use primarily on paper and paperboard.APPLICATIONS: ROVENE® 6101 can be used as a high gloss letdown vehicle for paper and paperboard substrates that provides high gloss and hold out, as well as excellent transfer and color development. ROVENE® 6101 can be easily formulated into inks and overprints varnishes using the standard product lines and additives used within the graphic arts industry.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0377 lb/in³
Solids Content 47 - 50 %
47 - 50 %
Particle Size <= 0.11 µm
<= 0.11 µm
Average
pH 8.1 - 8.8
8.1 - 8.8
Brookfield Viscosity 500 - 1800 cP
500 - 1800 cP
#2/20 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 104 °C
219 °F
Chemical Properties Metric English Comments
Total Acid Number 62
62
Calculated
Descriptive Properties Value Comments
Appearance Translucent Emulsion
Freeze/Thaw Stable 5 Cycles