Mallard Creek Polymers Rovene® 6115 Resin Supported Emulsion

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Mallard Creek Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers Rovene® 6115 Resin Supported Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Rovene® 6115 is a hard, non-film forming vehicle that is neutralized with sodium hydroxide for flexographic and gravure inks and overprint varnishes primarily for use on paper and paperboard substrates. Inks formulated with this emulsion exhibit excellent ink transfer as well as exceptional resolubility on press with low odor. Inks and overprint varnishes formulated with Rovene® 6115 dry fast, clean up easily on press, and can be easily formulated with graphic arts industry standard products and additives. Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Rovene® 6115 Material Safety Data Sheet before handling, storing, or using this product.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0377 lb/in³
Solids Content 48 - 50 %
48 - 50 %
pH 7.8 - 8.6
7.8 - 8.6
Brookfield Viscosity <= 1000 cP
<= 1000 cP
#20/200
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 105 °C
221 °F
Chemical Properties Metric English Comments
Total Acid Number 60
60
[mgKOH/g]