Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Malvern Minerals Diallylphthalate with Methallylate Silane Treated Novakup® 1250 Quartz Filler

Category Polymer , Thermoset , Diallyl Phthalate (DAP)
Manufacturer Malvern Minerals Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Malvern Minerals Diallylphthalate with Methallylate Silane Treated Novakup® 1250 Quartz Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product data demonstrates the effect of the Novakup® (lamellar quartz surface treated with 1.0% Z-6030 methallylate silane) filler. Separate entries demonstrate the effect of untreated Novacite® filler in DAP and vinyl silane surface treatment. The specific DAP used is Dapon 35 Resin.Information provided by Malvern Minerals Company.
Physical Properties Metric English Comments
Water Absorption 0.16 %
0.16 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 108
108
Flexural Strength 82.7 MPa
12000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 151 °C
304 °F
Heat Deflection, load unknown
Electrical Properties Metric English Comments
Insulation Resistance 6.00e+15 ohm
6.00e+15 ohm
Wet; after 16 hours at 130°C
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
Dry
3.8

@Frequency 1000 Hz
3.8

@Frequency 1000 Hz
Dry
3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
Wet
3.9

@Frequency 1000 Hz
3.9

@Frequency 1000 Hz
Wet
Dissipation Factor 0.0060

@Frequency 1.00e+6 Hz
0.0060

@Frequency 1.00e+6 Hz
Dry
0.0060

@Frequency 1.00e+6 Hz
0.0060

@Frequency 1.00e+6 Hz
Wet
0.010

@Frequency 1000 Hz
0.010

@Frequency 1000 Hz
Dry
0.017

@Frequency 1000 Hz
0.017

@Frequency 1000 Hz
Wet