Material Notes:
Product data demonstrates the effect of the Novacite® quartz filler. Separate entries demonstrate the effect of silane-treated Novakup® quartz filler in DAP. The specific DAP used is Dapon 35 Resin.Information provided by Malvern Minerals Company.
Physical Properties Metric English Comments
Water Absorption 0.16 %
0.16 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 106
106
Flexural Strength 65.5 MPa
9500 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 156 °C
313 °F
Heat Deflection, load unknown
Electrical Properties Metric English Comments
Insulation Resistance 3.60e+14 ohm
3.60e+14 ohm
Wet; after 16 hours at 130°C
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
Dry
3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
Wet
3.8

@Frequency 1000 Hz
3.8

@Frequency 1000 Hz
Dry
3.9

@Frequency 1000 Hz
3.9

@Frequency 1000 Hz
Wet
Dissipation Factor 0.0060

@Frequency 1.00e+6 Hz
0.0060

@Frequency 1.00e+6 Hz
Dry
0.0080

@Frequency 1000 Hz
0.0080

@Frequency 1000 Hz
Dry
0.0096

@Frequency 1.00e+6 Hz
0.0096

@Frequency 1.00e+6 Hz
Wet
0.019

@Frequency 1000 Hz
0.019

@Frequency 1000 Hz
Wet
Users viewing this material also viewed the following: