Manufacturing Insight EFR-4 Enhanced Fire Retardant Additive

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Manufacturing Insight LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Manufacturing Insight EFR-4 Enhanced Fire Retardant Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EFR-4 is ideal for incorporation into urethane resin systems, including coatings, foams and other similar applications.When blended into a resin system, EFR-4 will react to heat and/or flame by foaming and forming a thick, high yield char barrier. The char barrier will extinguish fire and prevent further flame spread. Additionally, the char foam insulates and protects the polymer substrate from heat and fire damage.EFR-4 is halogen-free, contains no metals, PBDEs, PBBs or other brominated compounds and does not evolve the highly toxic and corrosive gasses associated with many other fire retardants. EFR-4 is a RoHS/WEEE compliant material. EFR-4 functions at loading levels around 30% by weight but specific and individual product testing must be undertaken to qualify the formulation.
Physical Properties Metric English Comments
Solubility in Water <= 1.0 %
<= 1.0 %
At 170°F
Particle Mesh Size 325 Mesh
325 Mesh
100% through
Descriptive Properties Value Comments
Appearance Very fine free flowing white powder
Char Activation Temp 240-260°C
Char Forming Efficiency 99% Minimum
Purity 98% Minimum