Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Mar-Bal
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.90 - 2.10 g/cc
1.90 - 2.10 g/cc
ASTM D792
Bulk Factor 1.0
1.0
ASTM D1895
Water Absorption 0.17 %

@Time 86400 sec
0.17 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.00 - 0.0010 cm/cm
0.00 - 0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 60 - 65
60 - 65
ASTM D2583
Tensile Strength 31.0 - 37.9 MPa
4500 - 5500 psi
ASTM D638
Flexural Strength 68.9 - 82.7 MPa
10000 - 12000 psi
ASTM D790
Flexural Modulus 8.96 - 11.0 GPa
1300 - 1600 ksi
ASTM D790
Compressive Strength 138 - 152 MPa
20000 - 22000 psi
ASTM D695
Shear Strength 68.9 - 75.8 MPa
10000 - 11000 psi
ASTM D732
Izod Impact, Notched 2.67 - 3.20 J/cm
5.00 - 6.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Flammability, UL94 HB
HB
Descriptive Properties Value Comments
Listed File E80533 Yes