Material Notes:
Product Description: Master Bond Polymer System EP17HT-3 is a one part epoxy that fully cures in 2-3 minutes at 250-300°F. It is capable of service up to +400°F with excellent strength retention properties. Also, unlike many other one part epoxies, EP17HT-3 can be cured in sections up to ¼ inch thick. EP17HT-3 is 100% reactive and contains no solvents or diluents. As a one part system, it not only requires no mixing, but the working life is “indefinite”. It will not gel until heated above 200°F. EP17HT-3 has excellent electrical insulation characteristics, superior chemical resistance and outstanding physical properties. It is yellow to brown in color. There is a paste version called EP17HT-3ND2 as well as a slightly toughened formulation called Supreme 17HT-3 which offers enhanced resistance to thermal cycling and thermal and mechanical shock. Product Advantages: One part system; no mixing required; contains no solvents or diluentsSnap cure: Sets up in 20-30 seconds and fully cures in 2-3 minutes at 250-300°F Superior temperature resistance; serviceable up to +400°F Outstanding electrical insulation properties and chemical resistance Can cure in sections up to ¼ inch thick Easy application: Unlimited working life—will not set up at room temperatureInformation provided by MasterBond®
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Viscosity 80000 - 130000 cP
80000 - 130000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D >= 85
>= 85
Tensile Strength at Break >= 552 MPa
>= 80000 psi
Shear Strength >= 14.5 MPa
>= 2100 psi
tensile lap, aluminum to aluminum
Thermal Properties Metric English Comments
CTE, linear 4.00 - 5.00 µm/m-°C
2.22 - 2.78 µin/in-°F
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Glass Transition Temp, Tg 110 - 120 °C
230 - 248 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Dielectric Constant 4.8

@Frequency 60.0 Hz,
Temperature 25.0 °C
4.8

@Frequency 60.0 Hz,
Temperature 77.0 °F
Processing Properties Metric English Comments
Cure Time 1.80 - 3.00 min

@Temperature 149 °C
0.0300 - 0.0500 hour

@Temperature 300 °F
3.00 - 4.02 min

@Temperature 121 °C
0.0500 - 0.0670 hour

@Temperature 250 °F
Shelf Life 6.00 Month
6.00 Month
in original, unopened containers