Master Bond EP30 Optically Clear, Low Viscosity Two Component Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP30 Optically Clear, Low Viscosity Two Component Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond Polymer System EP30 is a low viscosity, two component epoxy system for high performance bonding, coating, sealing, potting and encapsulation. It readily cures at room temperature or more rapidly at elevated temperatures, and has a four to one mix ratio by weight. This adhesive is 100% reactive and does not contain any solvents or diluents.
Physical Properties Metric English Comments
Viscosity 400 - 500 cP

@Temperature 23.0 °C
400 - 500 cP

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min

@Temperature 93.3 °C
1.00 - 2.00 hour

@Temperature 200 °F
1080 - 1440 min

@Temperature 23.0 °C
18.0 - 24.0 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Code "A" Clear; "B" Clear
Mix Ratio By Weight 100/25
Set-Up Time, minutes 25-30
At Room Temperature