Master Bond EP30D-7 Flexibilized, Abrasion Resistant Epoxy System

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP30D-7 Flexibilized, Abrasion Resistant Epoxy System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond Polymer System EP30D-7 is a versatile two component flexibilized, urethane-modified epoxy featuring superior strength, toughness and abrasion resistance for high performance bonding, sealing, coating, potting and encapsulation applications. It combines the advantageous performance characteristics of epoxy resins such as strength, chemical resistance and adhesive qualities, with those of polyurethanes including toughness, abrasion resistance and flexibility.
Physical Properties Metric English Comments
Viscosity 40000 - 50000 cP

@Temperature 23.0 °C
40000 - 50000 cP

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Cure Time 120 - 150 min

@Temperature 93.3 °C
2.00 - 2.50 hour

@Temperature 200 °F
2160 - 2880 min

@Temperature 23.0 °C
36.0 - 48.0 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Code "A" Black; "B" Yellow
Mix Ratio By Weight 100/15
Set-Up Time, minutes 45-50
At Room Temperature