Material Notes:
Description: Master Bond Polymer Adhesive EP30P is a two component, transparent, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is formulated to cure readily at room temperature or more quickly at elevated temperatures. It has a 4 to 1 mix ratio by weight and contains no solvents or diluents. Master Bond Polymer System EP30P produces high strength, rigid bonds which are resistant to chemicals including water, oil, acids, and many organic solvents. It is serviceable over the wide temperature range of -60°F to + 250°F. It bonds well to a wide variety of substrates including metals, glass, ceramics, and many plastics, especially polycarbonates and acrylics. EP30P has low linear shrinkage upon cure as well as good optical clarity. The cured compound is also an outstanding electrical insulator. This, coupled with its low viscosity, makes it an excellent encapsulating and potting compound. EP30P is widely used in fiber optics, electro-optics, optical, and related industries. EP30P can be conveniently dispensed with a gun type mixing device. Product Advantages: Convenient mixing: 4 to one 1 by weight, low viscosity. Easy application: contact pressure only required for cure; adhesive spreads evenly and smoothly. Versatile cure schedules: ambient temperature cures or fast, elevated temperature cures as required. Forms high strength, rigid bonds to a wide variety of substrates, particularly glass, polycarbonates and acrylics. Good optical clarity. Exceptionally low shrinkage. Excellent electrical insulation properties. Low viscosity, ideal for potting and encapsulation. Outstanding chemical resistance to water, acids, bases and salts.Information provided by MasterBond®
Physical Properties Metric English Comments
Viscosity 400 cP
400 cP
Part B
1200 - 1400 cP
1200 - 1400 cP
mixed compound
1600 - 1800 cP
1600 - 1800 cP
Part A
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 65.5 MPa
>= 9500 psi
Tensile Modulus 2.76 GPa
400 ksi
Shear Strength 21.5 MPa
3120 psi
Bond, Al to Al, after 30 days water absorption
22.1 MPa
3200 psi
Bond, Al to Al, RT Cure
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Optical Properties Metric English Comments
Refractive Index 1.56
1.56
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Dielectric Strength 15.7 kV/mm

@Thickness 3.17 mm
400 kV/in

@Thickness 0.125 in
Processing Properties Metric English Comments
Cure Time 120 - 180 min

@Temperature 93.3 °C
2.00 - 3.00 hour

@Temperature 200 °F
1440 - 2880 min

@Temperature 23.9 °C
24.0 - 48.0 hour

@Temperature 75.0 °F
Pot Life 30 - 35 min
30 - 35 min
100 gram batch
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in unopened container
Descriptive Properties Value Comments
Mixing Ratio (A to B) 4/1
by weight