Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Master Bond EP33CLV Epoxy Resists Chemicals and High Temperatures

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP33CLV Epoxy Resists Chemicals and High Temperatures.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Master Bond EP33CLV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and excellent chemical resistance. It has a 100 to 70 mix ratio by weight and a very convenient one to one ratio by volume. This system cures readily at room temperature or more rapidly at elevated temperatures. To optimize its properties, the recommended cure schedule is overnight at room temperature followed by a post cure at 150-200°F for 2-3 hours. Once cured EP 33CLV has an exceptionally high temperature resistance, serviceable up to 450°F. It resists a range of chemicals including water, oils, fuels and many acids, bases and solvents—some even at higher temperatures. This low to moderate viscosity system bonds well to a wide variety of substrates including metal, glass, ceramics and many rubbers and plastics. It is a good electrical insulator. EP33CLV can be used for small to moderate encapsulation applications. It is 100% reactive and does not contain any diluents or solvents. The color of Part A is light amber, Part B is amber. It is widely used in electronic, electrical, aerospace and specialty OEM type applications where easy handling and high temperature are important considerations. Product Advantages: Convenient mixing: one to one ratio by volume. Easy application: contact pressure only required for cure; adhesive spreads evenly and smoothly. High temperature resistance up to 450°F. Very god chemical resistance. Excellent electrical insulation properties. Good adhesion to a wide variety of substrates.Information provided by MasterBond®
Physical Properties Metric English Comments
Viscosity 1500 - 3000 cP
1500 - 3000 cP
Part B
30000 - 70000 cP
30000 - 70000 cP
Part A
Mechanical Properties Metric English Comments
Hardness, Shore D 80 - 85
80 - 85
Tensile Strength at Break >= 75.8 MPa
>= 11000 psi
Tensile Modulus 2.76 GPa
400 ksi
Shear Strength >= 19.3 MPa
>= 2800 psi
Bond, Al to Al
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Dielectric Constant 3.6

@Frequency 60.0 Hz,
Temperature 25.0 °C
3.6

@Frequency 60.0 Hz,
Temperature 77.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min

@Temperature 93.3 °C
1.00 - 2.00 hour

@Temperature 200 °F
2880 - 4320 min

@Temperature 23.9 °C
48.0 - 72.0 hour

@Temperature 75.0 °F
Pot Life 60 - 90 min
60 - 90 min
100 gram batch
Shelf Life 12.0 Month

@Temperature 23.9 °C
12.0 Month

@Temperature 75.0 °F
in unopened container
Descriptive Properties Value Comments
Mixing Ratio (A to B) 1:1
by volume
100:70
by weight
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved