Master Bond MB250NT Low viscosity ethyl cyanoacrylate

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond MB250NT Low viscosity ethyl cyanoacrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond MB250NT is a single component ethyl cyanoacrylate type system. This rapid curing, high strength system is used primarily in applications where the ISO 10993-5 for low toxicity is specified. Cyanoacrylates are commonly referred to as super glues or instant adhesives. Their curing is dependent upon the humidity with the higher the level, the faster the rate of cure. Since the cure is typically fast, only minimal contact pressure is required for bonding. There is no mixing or heating required for curing. Depending upon the humidity and the substrates, MB250NT will typically set up within 10-40 seconds. MB250NT bonds well to a variety of substrates especially metals, composites, plastics and rubbers, especially in the shear mode.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Viscosity 100 - 110 cP
100 - 110 cP
mixed compound; thixotropic
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
Tensile Strength 34.5 MPa

@Temperature 23.9 °C
5000 psi

@Temperature 75.0 °F
Elongation at Break 2 - 3 %
2 - 3 %
Tensile Modulus 1.38 - 1.72 GPa

@Temperature 23.9 °C
200 - 250 ksi

@Temperature 75.0 °F
Thermal Properties Metric English Comments
CTE, linear 70.0 - 75.0 µm/m-°C
38.9 - 41.7 µin/in-°F
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1e+15 ohm-cm

@Temperature 25.0 °C
>= 1e+15 ohm-cm

@Temperature 77.0 °F
Dielectric Constant 3.6

@Frequency 1000 Hz,
Temperature 23.0 °C
3.6

@Frequency 1000 Hz,
Temperature 73.4 °F
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month
unopened containers
Descriptive Properties Value Comments
Appearance Colorless, transparent liquid