Description: Master Bond MasterSil 705C is an electrically conductive, one component, non-corrosive, carbon filled silicone for bonding, sealing and coating. This black colored paste like system cures readily at ambient temperatures upon exposure to humidity; the higher the level, the faster the rate of cure. MasterSil 705C has good electrical conductivity and is used primarily in applications involving static dissipation or EMI-RFI shielding. MasterSil 705C is also used when an electrically conductive system that is non-metallic is required. It retains typical silicone type flexibility and high temperature resistance. It is serviceable over the wide temperature range of -75°F to +400°F. MasterSil 705C will bond well to a wide variety of substrates including other silicone materials, particularly gasket materials. It is most effective when applied in thin sections. Another highly desirable property is a very fast tack free time of 3-7 minutes depending upon humidity. Key Features Carbon filled Electrically conductive Room temperature curing Serviceable from -75°F to +400°FInformation provided by MasterBond®
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Tensile Strength at Break 1.72 MPa
250 psi
Elongation at Break 230 %
230 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 50 - 100 ohm-cm
50 - 100 ohm-cm
Dielectric Constant 4.2

@Frequency 50.0 Hz,
Temperature 25.0 °C
4.2

@Frequency 50.0 Hz,
Temperature 77.0 °F
Dielectric Strength 33.5 kV/mm
850 kV/in
Processing Properties Metric English Comments
Cure Time 3.00 - 7.00 min
0.0500 - 0.117 hour
Tack-free time
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in original unopened containers
Descriptive Properties Value Comments
Appearance black