Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Master Bond Supreme 3AN One Component, Heat Curing Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name Supreme
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond Supreme 3AN One Component, Heat Curing Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Master Bond Polymer System SUPREME 3AN is a one component, heat cured epoxy adhesive and sealant, featuring high peel and shear strength along with excellent thermal conductivity and convenient handling. SUPREME 3AN cures readily at 250°F in 20-30 minutes; and at 300°F in 5-10 minutes. Minimum curing temperature is 235°F. Being a one part system, no mixing is required and the working life is unlimited as it never cures at room temperature. The shelf life is 6 months in original closed containers. Master Bond Polymer Adhesive SUPREME 3AN produces remarkably good bonds with both high shear and high peel strength for service over a wide temperature range of -100°F to +250°F. It offers very superior resistance to impact, thermal shock, vibration and stress fatigue cracking while maintaining the moisture, creep, corrosion and heat resistance typical of epoxy resin adhesives. Master Bond Adhesive SUPREME 3AN can be applied without sagging or dripping even on vertical surfaces. It is 100% reactive and does not contain any diluents or solvents. SUPREME 3AN forms high strength and exceptionally tough bonds which are remarkably resistant to severe thermal cycling and many chemicals including water, oil, fuels, and most organic solvents even upon prolonged exposures. Adhesion to metals, glass, ceramics, wood vulcanized rubbers and many plastics is excellent. The hardened adhesive has outstanding thermal conductivity and is also a superior electrical insulator. It is widely used in aerospace, electronic, electrical, computer, automotive and chemical applications especially where convenient handling and rapid curing along with outstanding physical properties all are of critical importance. Product Advantages: Single component system; no mixing needed prior to application. Ease of application; non drip application feature. Versatile and rapid cure schedules; as fast as 5-10 minutes at 300°F or 20-30 minutes at 250°F. High shear and peel strength to similar and dissimilar substrates over the remarkable wide temperature range of -100°F to +250°F. Good electrical insulating properties and chemical resistance. Superior resistance to thermal shock, impacts and stress fatigue cracking. Superior durability and dimensional stability. Outstanding thermal conductivity. Unlimited working life, minimal waste compared to two part systems.Information provided by MasterBond®
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Mechanical Properties Metric English Comments
Hardness, Shore D >= 75
>= 75
Tensile Modulus 3.10 GPa
450 ksi
Shear Strength >= 8.27 MPa
>= 1200 psi
Tensile, Al to Al
Peel Strength >= 1.75 kN/m
>= 10.0 pli
T-peel, Al to Al
Thermal Properties Metric English Comments
Thermal Conductivity 3.31 - 3.46 W/m-K
23.0 - 24.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Processing Properties Metric English Comments
Cure Time 5.00 - 10.000 min

@Temperature 149 °C
0.0833 - 0.16667 hour

@Temperature 300 °F
20.000 - 30.0 min

@Temperature 121 °C
0.33333 - 0.500 hour

@Temperature 250 °F
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in original closed containers
Descriptive Properties Value Comments
Appearance Gray