Master Bond UV10TKLO-2 UV Curable Compound for Aerospace Applications

Category Polymer , Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond UV10TKLO-2 UV Curable Compound for Aerospace Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Master Bond UV10TKLO-2 is a special one component UV curable epoxy modified system for high performance bonding, sealing and encapsulation. This system has passed rigorous testing to meet low outgassing specifications, as per NASA ASTM E-595. UV10TKLO-2 has high clarity and cures readily at room temperature when exposed to UV light. The ideal wavelengths for curing are 320-365 nm and the desired energy is 20-40 milliwatts per cm². The UV system is not inhibited by oxygen. UV10TKLO-2 offers resistance to water as well as to various acids, bases and solvents. The epoxy features superior physical strength properties and its service temperature range is from -60°F to +300°F. UV10TKLO-2 can be cured in thicker sections, up to 1/16 of an inch and can be easily “layered” to higher levels. Most significantly, the low outgassing properties enable this UV to be used in a wide array of optical, electro-optical and vacuum applications that until now have been “off limits” for UV curable epoxies. It should be noted that to optimize the outgassing properties, UV10TKLO-2 should be preheated to approximately 50°C for 15 minutes prior to use and then allowed to cool down to room temperature. UV10TKLO-2 is a first class electrical insulator. Product Advantages: One component: no mixing required. Exceptionally fast curing with UV light source. Not oxygen inhibited. High viscosity with excellent clarity and light transmission. Excellent physical strength, electrical insulation and chemical resistance profile. Meets NASA low outgassing test, ASTM E-595, specifications.Information provided by MasterBond®
Physical Properties Metric English Comments
Water Absorption <= 1.0 %
<= 1.0 %
1 week immersion
Viscosity 10000 - 20000 cP

@Temperature 40.0 °C
10000 - 20000 cP

@Temperature 104 °F
225000 - 275000 cP

@Temperature 25.0 °C
225000 - 275000 cP

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 80 - 85
80 - 85
Tensile Strength at Break >= 41.4 MPa
>= 6000 psi
Tensile Modulus >= 1.38 GPa
>= 200 ksi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Dielectric Constant 3.6

@Frequency 60.0 Hz,
Temperature 25.0 °C
3.6

@Frequency 60.0 Hz,
Temperature 77.0 °F
Processing Properties Metric English Comments
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in original unopened container