Material Notes:
Information provided by McDanel Advanced Ceramic Technologies
Physical Properties Metric English Comments
Bulk Density 5.92 g/cc
0.214 lb/in³
Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Flexural Strength 276 MPa
40000 psi
Compressive Strength 1772 MPa
257000 psi
Thermal Properties Metric English Comments
CTE, linear 11.3 µm/m-°C

@Temperature 20.0 - 1000 °C
6.28 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 2.00 W/m-K
13.9 BTU-in/hr-ft²-°F
2.00 W/m-K

@Temperature 800 °C
13.9 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Maximum Service Temperature, Air 2200 °C
3990 °F
no load
Component Elements Properties Metric English Comments
Al2O3 0.17 %
0.17 %
CaO 0.10 %
0.10 %
Fe2O3 0.030 %
0.030 %
K2O 0.0020 %
0.0020 %
MgO 0.010 %
0.010 %
Na2O 0.0060 %
0.0060 %
SiO2 0.40 %
0.40 %
TiO2 0.14 %
0.14 %
Y2O3 10.5 %
10.5 %
ZrO2 89 %
89 %