MetalTek C86300 High Tensile Manganese Bronze

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer MetalTek
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek C86300 High Tensile Manganese Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High strength and hardness copper-zinc alloy.Applications: Steel mill nuts, ordnance parts, worm gears.Information provided by MetalTekCast UNS C86300; Cast Grade C86300; Cast ASTM B271, B584, B148; Military MIL-C-15345-6; SAE 430B (Discontinued)
Mechanical Properties Metric English Comments
Hardness, Brinell 229
229
Tensile Strength, Ultimate >= 760 MPa
>= 110000 psi
Tensile Strength, Yield >= 415 MPa
>= 60200 psi
Elongation at Break >= 12 %
>= 12 %
Component Elements Properties Metric English Comments
Aluminum, Al 6.0 %
6.0 %
Copper, Cu 63 %
63 %
Iron, Fe 3.0 %
3.0 %
Manganese, Mn 3.0 %
3.0 %
Zinc, Zn 25 %
25 %