Material Notes:
Excellent seawater corrosion resistance combined with nearly twice the strength of common stainless steels.Applications: Offshore piping systems, couplings. Centrifuge, dewatering equipment. Pump, valve trim, pulp digesters Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 235
235
Tensile Strength, Ultimate >= 620 MPa
>= 89900 psi
Tensile Strength, Yield >= 415 MPa
>= 60200 psi
Elongation at Break >= 25 %
>= 25 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 21 - 23.5 %
21 - 23.5 %
Copper, Cu <= 1.0 %
<= 1.0 %
Iron, Fe 62.67 - 71.9 %
62.67 - 71.9 %
As Balance
Manganese, Mn <= 1.5 %
<= 1.5 %
Molybdenum, Mo 2.5 - 3.5 %
2.5 - 3.5 %
Nickel, Ni 4.5 - 6.5 %
4.5 - 6.5 %
Nitrogen, N 0.10 - 0.30 %
0.10 - 0.30 %
Silicon, Si <= 1.0 %
<= 1.0 %
Descriptive Properties Value Comments
Heat Treatment Sol. Anneal