MetalTek MTEK 304L Cast UNS J92500 Austenitic Stainless Steel

Category Metal , Ferrous Metal , Austenitic , Stainless Steel , Cast Stainless Steel , T 300 Series Stainless Steel
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 304L Cast UNS J92500 Austenitic Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
"300" series, general corrosion resistant alloyApplications: Nuclear, chemical and food processing. Valve and pump trim.Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 153
153
Tensile Strength, Ultimate >= 485 MPa
>= 70300 psi
Tensile Strength, Yield >= 205 MPa
>= 29700 psi
Elongation at Break >= 35 %
>= 35 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 17 - 21 %
17 - 21 %
Iron, Fe 63.47 - 75 %
63.47 - 75 %
As Balance
Manganese, Mn <= 1.5 %
<= 1.5 %
Nickel, Ni 8.0 - 12 %
8.0 - 12 %
Silicon, Si <= 2.0 %
<= 2.0 %
Descriptive Properties Value Comments
Heat Treatment Sol. Anneal