MetalTek MTEK 35-15 Cast UNS N08605 Heat Resistant Stainless Steel

Category Metal , Ferrous Metal , Heat Resisting , Stainless Steel , Cast Stainless Steel , T 300 Series Stainless Steel
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 35-15 Cast UNS N08605 Heat Resistant Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good strength at heat treating temperatures. Resists thermal shock of repeated heating and cooling.Applications: Dampers, pots, blades, rolls, door frames, retorts, rolling mill guides.Information provided by MetalTekCast UNS N08605; Cast Grade HT; Cast ASTM A297, A351, A608; Wrought UNS N83300; Wrought Grade 330
Mechanical Properties Metric English Comments
Hardness, Brinell 179
179
Tensile Strength, Ultimate >= 450 MPa
>= 65300 psi
Tensile Strength, Yield >= 235 MPa
>= 34100 psi
Elongation at Break >= 4.0 %
>= 4.0 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 980 °C
1800 °F
Component Elements Properties Metric English Comments
Carbon, C 0.35 - 0.75 %
0.35 - 0.75 %
Chromium, Cr 15 - 19 %
15 - 19 %
Iron, Fe 38.75 - 51.65 %
38.75 - 51.65 %
As Balance
Manganese, Mn <= 2.0 %
<= 2.0 %
Nickel, Ni 33 - 37 %
33 - 37 %
Silicon, Si <= 2.5 %
<= 2.5 %
Descriptive Properties Value Comments
Heat Treatment Not Heat Treated