MetalTek MTEK 35-45MA Heat Resistant Stainless Steel

Category Metal , Ferrous Metal , Heat Resisting , Stainless Steel , Cast Stainless Steel
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 35-45MA Heat Resistant Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MetalTek
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 450 MPa
>= 65300 psi
Tensile Strength, Yield >= 235 MPa
>= 34100 psi
Elongation at Break >= 5.0 %
>= 5.0 %
Component Elements Properties Metric English Comments
Carbon, C 0.35 - 0.47 %
0.35 - 0.47 %
Chromium, Cr 33 - 36 %
33 - 36 %
Iron, Fe 11.03 - 23.65 %
11.03 - 23.65 %
As Balance
Manganese, Mn <= 2.0 %
<= 2.0 %
Molybdenum, Mo <= 0.50 %
<= 0.50 %
Nickel, Ni 43 - 47 %
43 - 47 %
Niobium, Nb (Columbium, Cb) <= 1.0 %
<= 1.0 %
Silicon, Si <= 2.0 %
<= 2.0 %
Descriptive Properties Value Comments
Heat Treatment Not Heat Treated