MetalTek MTEK CZ-100 Cast UNS N02100 Severe Corrosion and Heat Resistant Alloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer MetalTek
Trade Name MTEK
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK CZ-100 Cast UNS N02100 Severe Corrosion and Heat Resistant Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Strong, tough and resistant to a wide range of industrial chemicals.Applications: Process equipment; food, pharmaceutical and chemical.Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 121
121
Tensile Strength, Ultimate >= 345 MPa
>= 50000 psi
Tensile Strength, Yield >= 125 MPa
>= 18100 psi
Elongation at Break >= 10 %
>= 10 %
Component Elements Properties Metric English Comments
Carbon, C <= 1.0 %
<= 1.0 %
Copper, Cu <= 1.25 %
<= 1.25 %
Iron, Fe <= 3.0 %
<= 3.0 %
Manganese, Mn <= 1.5 %
<= 1.5 %
Nickel, Ni >= 95 %
>= 95 %
Silicon, Si <= 2.0 %
<= 2.0 %
Descriptive Properties Value Comments
Heat Treatment Not Heat Treated