Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Michelman® Coating X300™ Plus Water based, moisture and water resistant coating

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Coating X300™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Coating X300™ Plus Water based, moisture and water resistant coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Water based, moisture and water resistant coating.Usage: Coating X300™ Plus provides high levels of water resistance and good moisture resistance for kraft paper with improved water resistance over Coating X300™. Coating X300™ Plus protects food products from excessive moisture, freezer burn, and sticking. Gluability with hot melt adhesives is excellent, but cold set gluing is not recommended.Application data: Coating X300™ Plus can be applied at the corrugator using a blade or rod coater.Coating X300™ products are typically used for: Produce boxes that require protection from damp fields, wet fruit/vegetables and shipping ice; Meat, poultry and frozen food boxes that require release and protection from moisture within the box; Bakery products that require release and Building products that need protection in transit and on the job siteFood Contact Information when manufactured in the USA:FDA: 175.105: Components of adhesives.176.170: Components of paper and paperboard in contact with aqueous and fatty foods.(Restricted) 176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.940 - 0.960 g/cc
0.940 - 0.960 g/cc
pH 8.5 - 10.5
8.5 - 10.5
Brookfield Viscosity 300 - 700 cP
300 - 700 cP
Spindle # 3, rpm 60
Viscosity Measurement 10 - 20
10 - 20
[sec], EZ cup, Cup # 2
Descriptive Properties Value Comments
Appearance White, semi-viscous liquid
Solids Type Synthetic