Michelman® Michem® Emulsion 39235 Nonionic high density polyethylene emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Michelman®
Trade Name Michem® Emulsion
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Emulsion 39235 Nonionic high density polyethylene emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nonionic high density polyethylene emulsionUsage: Michem® Emulsion 39235 is best used as an additive in water based coatings where improved slip, rub resistance, hardness and/or block resistance are needed. This wax emulsion can be used as an additive to paper coatings, wood coatings, metal coatings, overprint varnishes, floor polish and other markets where slip and hardness are required, without significant degradation of gloss.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamFood Contact Information when manufactured in USA and Singapore:FDA:175.105: Components of adhesives.176.180: Components of paper and paperboard in contact with dry foods.Food Contact Information when manufactured in Belgium:FDA:175.105: Components of adhesives.176.180: Components of paper and paperboard in contact with dry foods. (Restricted)Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.990 - 1.01 g/cc
0.990 - 1.01 g/cc
Volatiles 64.5 - 65.5 %
64.5 - 65.5 %
pH <= 7.0
<= 7.0
Recommended pH of system
9.0 - 10.5
9.0 - 10.5
Brookfield Viscosity 10 - 50 cP
10 - 50 cP
Spindle # 1, rpm 60
Descriptive Properties Value Comments
Appearance Translucent liquid
Emulsifier Charge Nonionic
Solids Type High Density Polyethylene