Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Michelman® Michem® Emulsion 93235 Nonionic polyethylene emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Michelman®
Trade Name Michem® Emulsion
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Emulsion 93235 Nonionic polyethylene emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 93235 is a phenol free additive best used in water based coatings where improved slip, rub resistance, hardness and/or block resistance is needed. Michem® Emulsion 93235 has proven very effective for mar resistance in floor polish formulations as well as mar resistance and shine in car polish formulations.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamWhen manufactured in Belgium product meets food contact regulations for: Europe: Euro. Res. AP(2004)1Germany: BfR Recommendation XXXVI (Restricted)Food Contact Information when manufactured in Belgium: FDA:175.105: Components of adhesives.176.170: Components of paper and paperboard in contact with aqueous and fatty foods. 176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.990 - 1.01 g/cc
0.990 - 1.01 g/cc
Volatiles 64.5 - 65.5 %
64.5 - 65.5 %
pH >= 7.0
>= 7.0
Recommended pH of system
8.5 - 10.5
8.5 - 10.5
Brookfield Viscosity <= 50 cP
<= 50 cP
Spindle # 1, rpm 60
Descriptive Properties Value Comments
Appearance Translucent liquid
Emulsifier Charge Nonionic
Solids Type High Density Polyethylene