Material Notes:
Description: Water based primer for extrusion coated resinsUsage: Michem® Flex P1853 is a primer for metal and paper substrates to promote adhesion to extrusion coated resins resulting in exceptionally high bond strength. Application Data: Michem® Flex P1853 may be applied via flexo, gravure or smooth roll coater. Dry thoroughly with hot, circulating air. May be used for in-line or off-line processes. Recommended application weight for film substrates is between 0.1 - 1.0 dry g/m2.Food Contact Information when manufactured in the USA: FDA:175.105: Components of adhesives. (Restricted) 175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted) 176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted) 176.180: Components of paper and paperboard in contact with dry foods. (Restricted)When manufactured in Belgium product meets food contact regulations for: Europe: Euro. Res. AP(2004)1 (Restricted) Germany: BfR Recommendation XIV (Restricted)and BfR Recommendation XXXVI (Restricted)Food Contact Information when manufactured in Beldium: FDA:175.105: Components of adhesives.175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted) 176.180: Components of paper and paperboard in contact with dry foods. (Restricted)Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.990 - 1.01 g/cc
0.990 - 1.01 g/cc
Volatiles 68 - 70 %
68 - 70 %
pH 7.5 - 8.5
7.5 - 8.5
Brookfield Viscosity <= 100 cP
<= 100 cP
Spindle # 1, rpm 60
Descriptive Properties Value Comments
Appearance White translucent liquid