Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mid-Mountain Materials CERMEX® MT1000 Needled Fiberglass Mat

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Fibers
Manufacturer Mid-Mountain Materials
Trade Name CERMEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mid-Mountain Materials CERMEX® MT1000 Needled Fiberglass Mat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CERMEX® MT1000 fiberglass mat is comprised of high purity, highly resilient E-Glass fibers. CERMEX® MT1000 is lightweight, strong, and highly efficient as insulation in most high heat environments for extended periods at elevated temperatures. The absence of organic or synthetic binders makes this product smoke-free on heat-up and allows the product to remain mechanically stable even after exposure to extreme temperatures. Needled and Felted Blanket.Information provided by Mid-Mountain Materials
Physical Properties Metric English Comments
Density 0.144 - 0.176 g/cc
0.00521 - 0.00637 lb/in³
Thickness 6350 microns
250 mil
12700 microns
500 mil
25400 microns
1000 mil
Thermal Properties Metric English Comments
Thermal Conductivity 0.0576 W/m-K

@Temperature 149 °C
0.400 BTU-in/hr-ft²-°F

@Temperature 300 °F
0.0721 W/m-K

@Temperature 260 °C
0.500 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.0937 W/m-K

@Temperature 371 °C
0.650 BTU-in/hr-ft²-°F

@Temperature 700 °F
Melting Point 1120 °C
2050 °F
Maximum Service Temperature, Air 538 °C
1000 °F
Continuous
816 °C
1500 °F
Short term
Descriptive Properties Value Comments
Roll Length (ft) 150
1/4"
45
1"
75
1/2"
Sound Absorption Coefficient (Sabin/ft2) 0.04 ±0.04
1/4" thick, 250 Hz
0.07 ±0.02
1/2" thick, 250 Hz
0.17 ±0.02
1/4" thick, 500 Hz
0.29 ±0.04
1" thick, 250 Hz
0.30 ±0.03
1/2" thick, 500 Hz
0.30 ±0.03
1/4" thick, 1000 Hz
0.68 ±0.03
1/4" thick, 2000 Hz
0.72 ±0.08
1/2" thick, 1000 Hz
0.86 ±0.03
1" thick, 500 Hz
0.92 ±0.03
1" thick, 2000 Hz
0.94 ±0.05
1/2" thick, 2000 Hz
0.94 ±0.05
1/4" thick, 4000 Hz
0.95 ±0.04
1" thick, 1000 Hz
0.95 ±0.05
1" thick, 4000 Hz
0.97 ±0.05
1/2" thick, 4000 Hz
Width (in) 60