Mid-Mountain Materials HYTEX® 400 Kevlar® Industrial Textile

Category Other Engineering Material , Composite Fibers , Polymer , Thermoset , Aramid
Manufacturer Mid-Mountain Materials
Trade Name HYTEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mid-Mountain Materials HYTEX® 400 Kevlar® Industrial Textile.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: HYTEX is the trademark for the textile products manufactured by Mid-Mountain Materials, Inc. Hytex high performance textile products are manufactured from various yarns of varying chemistry and in differing confiations (cloth, tape, sleeving, rope etc.). Mid-Mountain can design hybrid materials by blending most any combination of yarns.HYTEX 400 textiles are manufactured from various Kevlar yarns to produce end products specifically designed for combinations of high strength, high modulus, light weight, and moderate thermal resistance.Information provided by Mid-Mountain Materials.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Continuous
316 °C
600 °F
Short Term
Decomposition Temperature 427 °C
800 °F
Descriptive Properties Value Comments
Abrasion Resistance Fair
Acid Resistance Fair
Alkali Resistance Good
Color Yellow
Composition Aromatic Polyamide
Solvent Resistance Excellent
Sunlight & Aging Resistance Fair