Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Misumi Machinable SiO2-MgO Ceramic

Category Ceramic , Machinable Ceramic , Oxide , Magnesium Oxide , Silicon Oxide
Manufacturer Misumi
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Misumi Machinable SiO2-MgO Ceramic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MISUMI Corporation.
Physical Properties Metric English Comments
Density 2.50 g/cc
0.0903 lb/in³
Water Absorption 0.000 %
0.000 %
Mechanical Properties Metric English Comments
Flexural Strength 94.0 MPa
13600 psi
Thermal Properties Metric English Comments
CTE, linear 9.40 µm/m-°C

@Temperature 20.0 - 500 °C
5.22 µin/in-°F

@Temperature 68.0 - 932 °F
12.6 µm/m-°C

@Temperature 20.0 - 800 °C
7.00 µin/in-°F

@Temperature 68.0 - 1470 °F
Thermal Conductivity 1.46 W/m-K
10.1 BTU-in/hr-ft²-°F
Melting Point 1200 °C
2190 °F
Maximum Service Temperature, Air 1000 °C
1830 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
Dielectric Constant 6.00
6.00
Dielectric Strength 40.0 kV/mm
1020 kV/in
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved