Mitsui AURUM® JCF3030 Polyimide, Carbon Fiber/PTFE Filled  (discontinued **)

Category Polymer , Thermoplastic , Polyimide, Thermoplastic
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mitsui AURUM® JCF3030 Polyimide, Carbon Fiber/PTFE Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AURUM JCF3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AURUM JCF3030 offers a unique balance of mechanical, thermal, and tribological properties for outstanding performance in demanding automotive, business machinery, industrial equipment, aerospace, and semiconductor equipment applications. AURUM components offer excellent mechanical strength and toughness, dimensional stability, low outgassing, and exceptional radiation resistance. In addition, AURUM exhibits outstanding resistance to hydraulic, automotive, and many industrial fluids and solvents, a low coefficient of thermal expansion, creep resistance, and flame retardancy. AURUM JCF3030 withstands high PV levels and provides a low wear factor and low friction surface over a broad temperature range in lubricated environments.Applications: AURUM JCF3030 components are excellent replacements for metals, ceramics, and other plastics. High performance AURUM parts include: thrust washers and oil seal rings for automotive and off road vehicle transmissions, thermal insulators and stripper fingers for high-speed copiers, jet engine components, check valve balls, spline couplings, heat-resistant gears, vanes, wear strips, and valve seats. Other AURUM applications include carriers for aluminum hard disks and silicon wafers, journal bearings, and bearing retainers.Information provided by DuPont
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hrs @ 73°F; ASTM D570
Moisture Absorption at Equilibrium 0.090 %
0.090 %
73°F; 60 RH, 24hrs
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ASTM D955
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 420 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 788 °F
ASTM D1238
29 g/10 min

@Load 10.0 kg,
Temperature 420 °C
29 g/10 min

@Load 22.0 lb,
Temperature 788 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 170 MPa
24600 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Strength 230 MPa
33300 psi
ASTM D790
Flexural Modulus 10.802 GPa
1566.7 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 388 °C
730 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 246 °C
475 °F
ASTM D648
Glass Transition Temp, Tg 250 °C
482 °F
DSC