Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mitsui LUCANTâ„¢ HC-100 Synthetic Oil

Category Fluid , Lubricant
Manufacturer Mitsui Chemicals America
Trade Name LUCANT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mitsui LUCANTâ„¢ HC-100 Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LUCANT®, a hydrocarbon-based synthetic oil having no polar groups, is a co-oligomer of ethylene and -olefin. It possesses surpassing resistance to heat and cold and lower dependence of viscosity on temperature. Characteristics Non-volatile, colorless and transparent Excellent viscosity-temperature properties Low dependence of viscosity on temperature Excellent heat and oxidation stability Low pour point High flash and fire points Chemically stable, thus causing little or no metallic corrosion Applications Lubricant: Base oil and formulating ingredient for special lubricants, greases and functional fluids, which require resistance to heat and cold Rubber: Oil extender and processability improver in cases, which require resistance to heat, cold and volatility Resins: Softening and process agent Other: Pressure-sensitive adhesive, bonding agents, coating materials, ink, heat medium and special solutions Information provided by Mitsui Chemicals America, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.841 g/cc
0.841 g/cc
d<sup>20</sup><sub>4</sub>; Anton Paar density meter
Brookfield Viscosity 28000 cP

@Temperature 0.000 °C
28000 cP

@Temperature 32.0 °F
ASTM D2983
76000 cP

@Temperature -10.0 °C
76000 cP

@Temperature 14.0 °F
ASTM D2983
270000 cP

@Temperature -20.0 °C
270000 cP

@Temperature -4.00 °F
ASTM D2983
1.20e+6 cP

@Temperature -30.0 °C
1.20e+6 cP

@Temperature -22.0 °F
ASTM D2983
Viscosity Measurement 165
165
Viscosity Index; JIS K 2283
Kinematic Viscosity at 40°C (104°F) 1300 cSt
1300 cSt
JIS K 2283
Kinematic Viscosity at 100°C (212°F) 100 cSt
100 cSt
JIS K 2283
Ash <= 0.010 %
<= 0.010 %
JIS K 2272
ASTM Color 5.0
5.0
ASTM D1209
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 3.0
3.0
[kg/cm<sup>2</sup>]; 750 rpm; JIS K 2519
7.0
7.0
[kg/cm<sup>2</sup>]; 200 rpm; JIS K 2519
Thermal Properties Metric English Comments
Pour Point -32.5 °C
-26.5 °F
JIS K 2269
Flammability Test 320
320
[°C]; Fire Point; JIS K 2265
410
410
Autoignition temp.; ASTM D2155-66
Flash Point 280 °C
536 °F
COC Method; JIS K 2265
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Chemical Properties Metric English Comments
Acid Value <= 0.010
<= 0.010
[mg KOH/g]; total acid number; JIS K 2501
Descriptive Properties Value Comments
Aniline Point °C 160
JIS K 2265
Carbon Residue wt% 0.01
JIS K 2270
Copper Corrosion 1
JIS K 2513
Reaction Neutral
JIS K 2252