Material Notes:
Appearance: Solid clear borosilicate glass microspheres with white color in powder form.Typical applications of GL0179 beads include: calibration, high temperature spacer material for gauge control, coating, filler for plastic and etc.Information provided by Mo-Sci Corporation.
Physical Properties Metric English Comments
Bulk Density 1.20 g/cc
0.0434 lb/in³
of Dry Beads
Density 2.20 g/cc
0.0795 lb/in³
pH 7.0
7.0
in water
Mechanical Properties Metric English Comments
Compressive Strength 187.6 MPa
27210 psi
(Crush Strength) 90% Survival, using Carver Hydraulic Press
Thermal Properties Metric English Comments
CTE, linear 3.20 µm/m-°C

@Temperature 30.0 - 300 °C
1.78 µin/in-°F

@Temperature 86.0 - 572 °F
Softening Point 830 °C
1530 °F
Optical Properties Metric English Comments
Refractive Index 1.47 - 1.48
1.47 - 1.48
Component Elements Properties Metric English Comments
Al2O3 2.0 - 5.0 %
2.0 - 5.0 %
B2O3 10 - 15 %
10 - 15 %
Na2O 5.0 - 10 %
5.0 - 10 %
SiO2 70 - 85 %
70 - 85 %