Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials Electro 1700 Heat Cured Rubber - High Voltage Insulating

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials Electro 1700 Heat Cured Rubber - High Voltage Insulating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance standards.Electro 1700 is a specialty grade, platinum (addition/heat) curable silicone elastomer.Key Feature: Excellent Tracking and erosion resistance (1a 4.5KV); improved hydrophobicity
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength 5.20 MPa
754 psi
Elongation at Break 270 %
270 %
Tear Strength 20.0 kN/m
114 pli
Die B
Descriptive Properties Value Comments
Appearance Grey