Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials RTV116 One Component Acetoxy Adhesive Sealant, Red

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials RTV116 One Component Acetoxy Adhesive Sealant, Red.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. Acetic acid vapors are released from the sealant surface as a by-product of cure.RTV116 sealant is a self-leveling, standard strength high temperature sealant.Key Performance Properties: One-component productsCapability to cure at room temperature and ambient humiditySelf adhesion propertiesLow temperature flexibilityHigh temperature performanceExcellent weatherability and ozone and chemical resistanceExcellent electrical insulation propertiesApplications: Thin section potting, filling small surface voids, self leveling protective coating, electrical insulation where high temperature performance is required.FDA 21 CFR 177.2600 USDA NSF International Std. No. 51GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
Viscosity 25000 cP
25000 cP
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 20
20
Tensile Strength, Ultimate 2.45 MPa
356 psi
Elongation at Break 350 %
350 %
Adhesive Bond Strength 0.686 MPa
99.5 psi
At 100% cohesive failure
Peel Strength 4.38 kN/m
25.0 pli
At 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle
Thermal Properties Metric English Comments
CTE, linear 270 µm/m-°C

@Temperature 20.0 °C
150 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C
500 °F
Continuous
315 °C
599 °F
Intermittent
Brittleness Temperature -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
Dielectric Constant 2.8

@Frequency 60 Hz
2.8

@Frequency 60 Hz
Dielectric Strength 16.0 kV/mm
406 kV/in
Dissipation Factor 0.0010

@Frequency 60 Hz
0.0010

@Frequency 60 Hz
Processing Properties Metric English Comments
Cure Time 30 min
0.5 hour
Tack-free
Descriptive Properties Value Comments
Color Red
Consistency Self-leveling