Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials Siloprenâ„¢ LSR 2345/07 Liquid Silicone Rubber - Specialty Coating

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name Silopren™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials Siloprenâ„¢ LSR 2345/07 Liquid Silicone Rubber - Specialty Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conductive coating - Physical Properties are subject to the substrate that is used.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.027 cm/cm
0.027 in/in
vulcanized 10 sec at 200°C; Without post-cure
0.035 cm/cm
0.035 in/in
vulcanized 10 sec at 200°C then post-cured
Electrical Properties Metric English Comments
Surface Resistance 230 ohm

@Diameter 0.150 mm
230 ohm

@Diameter 0.00591 in
Processing Properties Metric English Comments
Nozzle Temperature 20.0 °C
68.0 °F
cool nozzle and cylinder to prevent premature vulcanization
Mold Temperature 140 - 230 °C
284 - 446 °F
short vulcanization time required (a few seconds)
Injection Pressure 5.00 - 15.0 MPa
725 - 2180 psi
depends on feed channel
Hold Pressure 5.00 MPa
725 psi
Descriptive Properties Value Comments
Appearance Black
Copyright © lookpolymers.com All Rights Reserved