Momentive Performance Materials TSE 221-6U Heat Cured Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials TSE 221-6U Heat Cured Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance standards.TSE 221-6U is a peroxide curable, general purpose silicone elastomer.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength 7.30 MPa
1060 psi
Elongation at Break 280 %
280 %
Tear Strength 18.0 kN/m
103 pli
Die B
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB
Descriptive Properties Value Comments
Appearance Light Grey