Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials TSE322 Heat-Curing Silicone Adhesive, Light Blue

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials TSE322 Heat-Curing Silicone Adhesive, Light Blue.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RTV6424, RTV6445, and TSE322 silicone adhesives are one-component heat curable silicone adhesive sealants which will bond to many substrates without a primer and which will creep rapidly at elevated temperatures. These products have a very long working time at room temperature but will not cure completely until exposed to elevated temperatures. TSE322 is a light blue, flowable material with self-leveling properties.Mechanical properties for specimen cured 1 hour at 150°C.Key Performance Properties: One component product - no mixing requiredFast cure at elevated temperaturePrimerless adhesion to many types of substratesNo cure by-products, low linear shrinkageExcellent dielectric propertiesOutstanding performance over a wide thermal range.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
Viscosity 150000 cP
150000 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
Tensile Strength, Ultimate 2.930 MPa
425.0 psi
Elongation at Break 200 %
200 %
Adhesive Bond Strength 2.07 MPa
300 psi
Aluminum to aluminum
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Constant 3.1
3.1
Dielectric Strength 19.69 kV/mm
500.1 kV/in
Dissipation Factor 0.0060
0.0060
Descriptive Properties Value Comments
Color Light Blue
Users viewing this material also viewed the following: