Material Notes:
DOW CORNING 4-7051 Siloxane Powder Resin Modifiers are 100% active, free-flowing, siloxane powders. They are available in several grades with varying types of organic reactivity processing thermoplastics. They can modify the burning characteristics of thermoplastics, reducing the rate of heat release and the rate of smoke and carbon monoxide evolution. Similar burning characteristic modifications have been observed in halogen-free, halogenated and phosphorus flame retardant systems.Information provided by Multibase, a Dow Corning Company
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc

@Temperature 25.0 °C
1.20 g/cc

@Temperature 77.0 °F
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Color White
Physical Form Coarse Powder
Copyright © lookpolymers.com All Rights Reserved