Material Notes:
Moisture content is 0.08%.Data provided by Multibase.
Physical Properties Metric English Comments
Melt Flow 5.8 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.8 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 37.5 MPa
5440 psi
ASTM D638-95
Elongation at Break 35.3 %
35.3 %
ASTM D638-95
Flexural Strength 60.0 MPa
8700 psi
ASTM D790-95
Flexural Modulus 2.232 GPa
323.7 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256-93a
Gardner Impact 1.80 J
1.33 ft-lb
ASTM D5420-93