Material Notes:
Features: Chemical Resistance, GoodCompressive Strength, GoodHeat Resistance, MediumOzone ResistantThermal Stability, GoodForms:PelletsProcessing Methods:Injection MoldingExtrusion Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM 792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 33
33
10 seconds; ASTM D2240
Tensile Strength, Yield 0.827 MPa
120 psi
at 100% secant; ASTM D412
5.52 MPa
800 psi
Elastic; ASTM D412
Elongation at Break 600 %
600 %
Elastic; ASTM D412
Tear Strength 17.5 kN/m
100 pli
ASTM D624
Compression Set 11 %
11 %
73°F, 70 hours; ASTM D395
39 %
39 %
158°F, 70 hours; ASTM D395
Processing Properties Metric English Comments
Middle Barrel Temperature 210 °C
410 °F
Front Barrel Temperature 227 °C
440 °F
Nozzle Temperature 235 °C
455 °F
Mold Temperature 51.7 °C
125 °F
Moisture Content <= 0.060 %
<= 0.060 %
Users viewing this material also viewed the following: