Multibase Multi-Flex® A 5003 TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 5003 TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good General PurposeHardness, MediumForms:PelletsProcessing Method:Extrusion Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM 792
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
ASTM D955
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 46
46
10 seconds; ASTM D2240
Tensile Strength, Yield 8.27 MPa
1200 psi
Elastic; ASTM D412
Elongation at Break 630 %
630 %
Elastic; ASTM D412
Tear Strength 29.8 kN/m
170 pli
ASTM D624
Compression Set 33 %
33 %
73°F, 70 hours; ASTM D395
68 %
68 %
158°F, 70 hours; ASTM D395
Processing Properties Metric English Comments
Melt Temperature 191 - 204 °C
375 - 400 °F
Mold Temperature 125 °C
257 °F