Multibase Multi-Flex® A 6041 Clear TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 6041 Clear TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This material bonds to polypropylene.Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.892 g/cc
0.892 g/cc
ASTM 792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 91 g/10 min

@Load 2.16 kg,
Temperature 230 °C
91 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 59
59
10 seconds; ASTM D2240
Tensile Strength at Break 7.45 MPa
1080 psi
ASTM D412
Elongation at Break 730 %
730 %
ASTM D638
Tear Strength 43.8 kN/m
250 pli
ASTM D624
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Middle Barrel Temperature 210 °C
410 °F
Front Barrel Temperature 227 °C
440 °F
Nozzle Temperature 235 °C
455 °F
Mold Temperature 51.7 °C
125 °F