Material Notes:
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.982 g/cc
0.982 g/cc
ASTM 792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
10 seconds; ASTM D2240
Tensile Strength, Yield 11.7 MPa
1700 psi
Elastic; ASTM D412
Elongation at Break 730 %
730 %
Elastic; ASTM D412
Flexural Modulus 0.0965 GPa
14.0 ksi
1% Secant; ASTM D790
Tear Strength 57.8 kN/m
330 pli
ASTM D624
Processing Properties Metric English Comments
Middle Barrel Temperature 210 °C
410 °F
Front Barrel Temperature 227 °C
440 °F
Nozzle Temperature 235 °C
455 °F
Mold Temperature 51.7 °C
125 °F