Multibase Multi-Flex® D 6606 TPO Thermoplastic Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyolefin
Manufacturer Multibase
Trade Name Multi-Flex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® D 6606 TPO Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Chemical Resistance, Good PaintableOzone ResistantDensity, LowTear Strength, GoodUV Resistance, GoodStiffness, Good Forms:PelletsUses: Automotive ApplicationsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM 792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
10 seconds; ASTM D2240
Tensile Strength, Yield 15.2 MPa
2200 psi
Elastic; ASTM D638
Elongation at Break 150 %
150 %
ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Tear Strength 92.9 kN/m
530 pli
ASTM D624
Processing Properties Metric English Comments
Rear Barrel Temperature 177 - 199 °C
350 - 390 °F
Middle Barrel Temperature 199 - 221 °C
390 - 430 °F
Front Barrel Temperature 221 - 232 °C
430 - 450 °F
Nozzle Temperature 6.11 - 232 °C
43.0 - 450 °F
Melt Temperature 232 °C
450 °F
Mold Temperature 37.8 °C
100 °F
Descriptive Properties Value Comments
Clamp Tonnage 2-4 tons/in2
Screw L/D Ratio 20:1
Copyright © lookpolymers.com All Rights Reserved