Material Notes:
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM 792
Melt Flow 2.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
10 seconds; ASTM D2240
Tensile Strength, Yield 4.23 MPa
613 psi
Elastic; ASTM D412
0.979 MPa

@Strain 100 %
142 psi

@Strain 100 %
ASTM D412
Elongation at Break 780 %
780 %
Elastic; ASTM D412
Tear Strength 17.5 kN/m
100 pli
ASTM D624
Compression Set 15 %
15 %
73°F, 70 hours; ASTM D395
38 %
38 %
158°F, 70 hours; ASTM D395
Thermal Properties Metric English Comments
Flame Spread 51 mm/min
2.0 in/min
FM VSS-302