Multibase Multi-Flex® TPE A 3104-10 AGATE 5ES

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 3104-10 AGATE 5ES.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The material is based on Kraton G rubber. It has been engineered for single shot. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore D 38
38
10 sec; ASTM D-2240
Tensile Strength, Ultimate 12.0 MPa
1740 psi
ASTM D412
Elongation at Break 580 %
580 %
ASTM D412
Flexural Modulus 0.232 GPa
33.6 ksi
ASTM D790-92
Tear Strength 77.0 kN/m
439 pli
ASTM D624