Multibase Multi-Flex® TPE A 5009

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 5009.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Physical Properties Metric English Comments
Melt Flow 9.0 g/10 min
9.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
10 sec; ASTM D-2240
Tensile Strength, Ultimate 11.9 MPa
1730 psi
ASTM D638
Elongation at Break 850 %
850 %
ASTM D638
Flexural Modulus 0.370 GPa
53.7 ksi
at RT method 1, proc. B; ASTM D-790
Gardner Impact 28.2 J
20.8 ft-lb
ASTM D1709
Tear Strength 74.4 kN/m
425 pli
(Die C) ASTM D-624