Material Notes:
The data is the actual data obtained from the above sample. This material is based on Shell's Kraton G technology. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.997 g/cc
0.0360 lb/in³
ASTM D792
Melt Flow 2.35 g/10 min
2.35 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
10 sec; ASTM D-2240
Tensile Strength, Ultimate 8.80 MPa
1280 psi
ASTM D412
Elongation at Break 795 %
795 %
ASTM D412
Tear Strength 41.2 kN/m
235 pli
ASTM D624
Compression Set 30 %
30 %
for 168 hours at 25°C; ASTM 395