Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPE D 5010

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE D 5010.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.87 g/cc
0.0676 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 15 g/10 min
15 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
10 sec; ASTM D-2240
Tensile Strength, Ultimate 7.50 MPa
1090 psi
ASTM D412
Elongation at Break 200 %
200 %
ASTM D412
Flexural Modulus 0.508 GPa
73.7 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 42.3 kN/m
241 pli
ASTM D624
Copyright © lookpolymers.com All Rights Reserved